Here are some pics of my latest firing results from my gas kiln. I take it to Cone 10 and start reduction at 750 degrees C and keep it there til I reach temperature. I’m getting much better results largely due to my concentrated effort to NOT put runny glazes on the back!! and to avoid using too many test glazes all over pieces (I really don’t know why that would be a struggle!).
I also got lots of great copper reds, but I’ll put them in a separate post.
Get to glazing!
Love,
Marian
I love the tea dust over temmoku. Is that sprayed over or do you use a resist. Cool
Hi, Kate,
It is usually sprayed. Sometimes I dip an edge as it is super fluid and runny. Glad you love it!
All the best,
Marian
Love your Chun glaze! Would you be willing to share your recipe?
Hi, thanks, it is a good one. Unfortunately, I can’t share it, but it is a pretty standard chun. Thanks for reading and commenting!
All the best,
Marian